Metallurgy for Wear parts VSI

Posted in: , on 26. Mar. 2009 - 09:16

Hi,

We are using a vertical shaft impactor for a material which consists of silica 89% and Mgo 0.45%. We are presently using tungsten carbide tips and also ni hard liners. These are hardly coming for 100 hours and wearing out very fast. Could any one suggest a suitable mettalurgy for the wear parts.

We are feeding -25 mm and taking out -4.75 mm. The SG of material is 2.75

Regards

H. Sankaranarayanan

VP Operations

Taurian Iron & Steel co. pvt ltd

Mumbai

h.sankar@tauriansteel.com

Write the first Reply